Abstract The pulsed CO2 laser cutting experiment of 2A12 aluminum alloy is carried out to study the morphology and element of fracture surface as well as the size and microstructure of hear affected zone. Then, compared with water-jet cutting, the influences of heat affected zone on single-direction tesile properties and fatigue life of specimen are analyzed, and the factigue fracture is studied using microscope.
|
|
|
|
|